Styron XZ 97217.00 Styrene Acrylate

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XZ 97217.00 Styrene Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Performance Features: For use in D1 building adhesive formulationsApplications: Waterproofing Membranes and MasticsEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 49 %
49 %
pH 8.0
8.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 22.0 °C
71.6 °F