Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sylvin Technologies 8925-60 Natural PVC Extrusion Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Sylvin Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 8925-60 Natural PVC Extrusion Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 seconds
Tensile Strength, Ultimate 9.65 MPa
1400 psi
Elongation at Break 480 %
480 %
Tear Strength Test 190
190
Processing Properties Metric English Comments
Melt Temperature 154 - 166 °C
310 - 330 °F