Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength at Break 29.42 MPa
4267 psi
Elongation at Break 900 %
900 %
100% Modulus 0.00440 GPa
0.638 ksi
300% Modulus 0.00590 GPa
0.856 ksi
Resilience 50
50
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 25
25
Processing Properties Metric English Comments
Feed Temperature 165 °C
329 °F
Middle Barrel Temperature 170 °C
338 °F
Compress zone
Front Barrel Temperature 175 °C
347 °F
Metering zone
Adapter Temperature 180 °C
356 °F
Die Temperature 180 °C
356 °F