| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Carbon Fiber/PTFE Filled |
| Manufacturer | Techmer ES |
| Trade Name | Plaslube® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
| Water Absorption | 0.70 % | 0.70 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 152 MPa | 22000 psi | ASTM D638 |
| Elongation at Break | 2.5 % | 2.5 % | ASTM D638 |
| Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
| Flexural Modulus | 8.96 GPa | 1300 ksi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1000 - 10000 ohm-cm | 1000 - 10000 ohm-cm | ASTM D648 |
| Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |