Techmer ES Plastiblend® PC/ABS FR GF30 30% Glass Filled

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® PC/ABS FR GF30 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 117 MPa
16900 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Yield Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.4 µm/m-°C
23.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB