Teknor Apex APEX® 3703-75NT1 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 3703-75NT1 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Non-Phthalate - TOTM Plasticizer Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
10 seconds; ASTM D2240
Tensile Strength at Break 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 410 %
410 %
ASTM D638
Descriptive Properties Value Comments
Appearance Clear