Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Monprene® MP 1875 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Teknor Apex Company
Trade Name MONPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Monprene® MP 1875 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: Water; Clear; Adhesion to Polycarbonate Features: High Coefficient of FrictionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 3.00 g/10 min

@Load 2.16 kg,
Temperature 150 °C
3.00 g/10 min

@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
ASTM D412
Tensile Strength, Yield 3.45 MPa

@Strain 300 %
500 psi

@Strain 300 %
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412