Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
5 seconds; ASTM D2240
Tensile Strength, Yield 2.76 MPa
400 psi
Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412
4.69 MPa
680 psi
85% Retention, Hot Air Aging, 22 hrs at 70°C
5.52 MPa
800 psi
ASTM D412
Elongation at Break 320 %
320 %
80% Retention; Hot Air Aging, 22 hrs at 70°C
400 %
400 %
ASTM D412
Elongation at Yield 100 %
100 %
Adhesion to EPDM, 0.125" Micro Die, 8"/min; ASTM D412
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Compression Set 29 %
29 %
23°C, 22 hr.; ASTM D395, Method B
42 %
42 %
70°C, 22 hr.; ASTM D395, Method B