Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Thermoseal KLINGERSIL® C-4408 Metal Reinforced Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Thermoseal Inc.
Trade Name KLINGERSIL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal KLINGERSIL® C-4408 Metal Reinforced Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Synthetic FiberNitrile BinderHigh Temperature & StressFluctuating Temperatures & PressuresVibrationLow Carbon Steel Woven Mesh InsertInformation provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM F1315
Thickness 1588 microns
62.52 mil
Thickness tested
Descriptive Properties Value Comments
Color Black
(Top/Bottom)
Compressibility 8 percent
ASTM F36J
Creep Relaxation 20 percent
1/32", ASTM F38B
Klinger Hot Compression Test 10 percent
Initial, Thickness Decrease 73°F (23°C)
22 percent
Additional, Thickness Decrease 572°F (300°C)
Recovery >50 percent
ASTM F36J
Thickness Increase 0-5%
ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
0-5%
ASTM Oil IRM903, 5h/300°F (149°C)
0-5%
ASTM Fuel A, 5h/73°F (23°C)
0-5%
ASTM Fuel B, 5h/73°F (23°C)
Weight Increase <10%
ASTM F146 after immersion in Fuel B 5h/73°F (23°C)