Material Notes:
Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D 792
Water Vapor Transmission 10.86 g/m²/day
0.6994 g/100 in²/day
E 96/66
Thickness 25.4 microns
1.00 mil
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
High Load Melt Index 20 g/10 min

@Load 21.6 kg
20 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 24.1 MPa
3500 psi
ASTM D 882 A
Film Tensile Strength at Yield, TD 24.1 MPa
3500 psi
ASTM D 882 A
Film Elongation at Break, MD 600 %
600 %
ASTM D 882 A
Film Elongation at Break, TD 700 %
700 %
ASTM D 882 A
Elmendorf Tear Strength MD 50 g
50 g
ASTM D 1922
Elmendorf Tear Strength TD 500 g
500 g
ASTM D 1992
Dart Drop Test 130 g
0.287 lb
ASTM D 1709 A
Film Tensile Strength at Break, MD >= 40.7 MPa
>= 5900 psi
ASTM D 882A
Film Tensile Strength at Break, TD >= 34.5 MPa
>= 5000 psi
ASTM D 882 A
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ASTM D3417