UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
ASTM D412
Tensile Strength at Break 18.5 MPa
2680 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.00230 GPa
0.334 ksi
ASTM D412
200% Modulus 0.00560 GPa
0.812 ksi
ASTM D412
300% Modulus 0.0102 GPa
1.48 ksi
ASTM D412
Rebound 60 %
60 %
BS.903,PART22
Tear Strength 51.0 kN/m
291 pli
ASTM D624
Abrasion 108
108
Lombourn Abrasion Index (Iwamoto Seisakusyo, Japan); UBE Method
228
228
Pico Abrasion Index; ASTM D2228
Compression Set 14 %
14 %
Method B, 70°C, 72hrs; ASTM D395
Descriptive Properties Value Comments
Cut Generation De Mattia Flexing Machine Min 300,000 times
ASTM D430
Cut Growth (2mm-->15mm)  De Mattia Flexing Machine 2400 times
ASTM D313
Goodrich Flex,  0.175" Stroke, 55lb, 100°C, P.S. 6%
ASTM D623 (29°C change in temperature)
Wet Skid Resistance on Safety-Walk 18
UBE Method (British Portable Skid Resistance Tester)