Unifrax Fiberfrax® HSA (OF) Ceramic Fiber Paper

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® HSA (OF) Ceramic Fiber Paper.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HSA paper is made from high surface area (HSA) fibers that contain a low percentage of unfiberized material. Use of this fiber results in a paper with lighter weight and extremely low thermal conductivity, making it the choice of the aerospace industry. It is also used when uniform pore structure and a low content of unfiberized material are required in applications such as glass contact or gas filtration. The HSA "OF" designation signifies materials made without the use of organic binders.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.112 g/cc
0.00405 lb/in³
Loss On Ignition 0.10 %
0.10 %
including binder
Thermal Properties Metric English Comments
Melting Point 1704 °C
3099 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 47 - 52 %
47 - 52 %
Fe2O3 <= 0.050 %
<= 0.050 %
SiO2 47 - 52 %
47 - 52 %
Descriptive Properties Value Comments
Color White
Fiber Index (% Wt) 100
Na2O3 (%) <0.5
Temperature Grade (°C) 1260