Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unipetrol C4 Fraction

Category Fluid , Solvent
Manufacturer Unipetrol RPA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol C4 Fraction.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
C4 fraction is a mixture of liquified hydrocarbons with prevailing content of 4 C atoms in their molecules. It is manufactured by fractional distillation of pyrolysis gases from thermal cracking of oil fractions. It is an easily volatile, flammable and combustible substance of characteristic odour.Information provided by Unipetrol RPA
Descriptive Properties Value Comments
Composition max. 0.0005
max. 0.015
max. 0.1
max. 0.3
max. 0.7
max. 1.5
max. 10
min. 0.005
min. 40
min. 65
Material 1,3 - Butadiene
1,3 - Butadiene and Isobutene
C3 and lower hydrocarbons
C4 Saturated Hydrocarbons
C5 and higher hydrocarbons
Carbonyls
Ethylacetylene and Vinylacetylene
Methylacetylene
Stabilizer
Sulfur
Users viewing this material also viewed the following: