Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake EF606 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EF606 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and is an excellent bubble stabilizer in LLDPE rich blends.Application/UsesTrash bagsGeneral purpose linersMultiwall linersIndustrial linersFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 50.8 microns
2.00 mil
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Dart Drop 4.92 g/micron
125 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
ASTM D882
1% Secant Modulus, MD 152 MPa
22000 psi
ASTM D882
1% Secant Modulus, TD 193 MPa
28000 psi
ASTM D882
Processing Properties Metric English Comments
Melt Temperature 182 - 204 °C
360 - 400 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution