Westlake Epolene® E-25 Chemically Modified Polypropylene, Maleation Processed

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® E-25 Chemically Modified Polypropylene, Maleation Processed.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Epolene E-25 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emulsions. Because of the polarity and anhydride functionality, Epolene E-25 is useful for laminating, as a compatibilizer for PP blends with nylon or EVOH, and for enhancing the strength of composites that utilize reinforcements / fillers such as glass, talc, calcium carbonate, and metals. Key Attributes: Coupling agent and compatibilizer for PP composites and alloysExcellent pigment dispersion aiMaleic anhydride grafted polypropylene (PP)Provides slip resistance in floor polish finishesUseful in adhesive blendsApplication/Uses:AutomotiveBookbindingBuilding and ConstructionCaulks and SealantsHot Melt AdhesivesLaminatingSolvent borne AdhesivesWaterborne Adhesives
Physical Properties Metric English Comments
Viscosity 150 - 700 cP

@Temperature 190 °C
150 - 700 cP

@Temperature 374 °F
542-130
Brookfield Viscosity 300 cP

@Temperature 190 °C
300 cP

@Temperature 374 °F
Molecular Weight 12000 g/mol
12000 g/mol
Thermal Properties Metric English Comments
Ring & Ball Softening Point 157 °C
315 °F
ASTM E28
Optical Properties Metric English Comments
Gardner Color Number 9.0
9.0
<= 11
<= 11
542-111
Chemical Properties Metric English Comments
Total Acid Number 25
25
Descriptive Properties Value Comments
Penetration Hardness <1 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm