175°C high-temperature service and excellent oil resistance.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Gehman T100
Descriptive Properties Value Comments
% Volume Swell 11
Curesite Chlorine
Users viewing this material also viewed the following: