Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zircar Zirconia CeF-100 Ceria Felt Insulation

Category Ceramic , Machinable Ceramic , Oxide
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Zirconia CeF-100 Ceria Felt Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ceria (cerium dioxide), CeO2, has a very high surface area and is ideal as a catalyst support. Our ceria fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia textiles. Our high purity ceria fiber and textiles are offered in six different standard product forms; bulk fiber Type CeBF, two felts Types CeF- 50 and CeF-100 and three types of knit cloth Types CeK-15, CeW-15 and CeW-30.Features: High PurityHigh Temperature Stability Low Thermal ConductivityExcellent Thermal Shock ResistanceNo OutgassingSix Different Product Formats OfferedAvailable ‘Off the Shelf’Application Information: Ceria Bulk Fiber and Felt are used in molten carbonate fuel cells. Ceria Knit Cloth is used for product development of gas sensors.Information provided by Zircar Zirconia.
Physical Properties Metric English Comments
Bulk Density 0.270 g/cc
0.00975 lb/in³
Loss On Ignition 0.300 %

@Temperature 950 °C,
Time 3600 sec
0.300 %

@Temperature 1740 °F,
Time 1.00 hour
Porosity 96 %
96 %
Bulk
Outgassing - Total Mass Loss 0.00 %
0.00 %
Thermal Properties Metric English Comments
Melting Point 2590 °C
4690 °F
Shrinkage 6.00 %

@Temperature 1650 °C,
Time 3600 sec
6.00 %

@Temperature 3000 °F,
Time 1.00 hour
Component Elements Properties Metric English Comments
Al2O3 0.050 %
0.050 %
CeO2 >= 99 %
>= 99 %
Fe2O3 0.030 %
0.030 %
SiO2 0.040 %
0.040 %
Descriptive Properties Value Comments
Tensile Strength per Unit Width 28 gram/cm width