Aaron Industries Corporation
Trade Name AAROPRENE® GFN
Trade Name :
AAROPRENE® GFN
Product List
Category
Nylon 66, 10% Glass Fiber Filled
,
Nylon 6, 30% Glass Fiber Filled
,
Nylon 66, 30% Glass Fiber Filled
Manufacturer
Aaron Industries Corporation
Tips:
Up to 50 items displayed.
PRODUCT NO.
Category
Aaron Industries AAROPRENE® GFN 6613 Glass Filled Nylon 6/6
Nylon 66, 10% Glass Fiber Filled
Aaron Industries AAROPRENE® GFN 6013 Glass Filled Nylon 6
Nylon 6, 10% Glass Fiber Filled
Aaron Industries AAROPRENE® GFN 6033 Glass Filled Nylon 6
Nylon 6, 30% Glass Fiber Filled
Aaron Industries AAROPRENE® GFN 6633 Glass Filled Nylon 6/6
Nylon 66, 30% Glass Fiber Filled