ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Trade Name :
Dryflex®
Product List
Category
Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
ELASTO UK Ltd, a Hexpol company
Tips:
Up to 50 items displayed.
PRODUCT NO.
Category
ELASTO UK Dryflex® 3021-001 TPE, Modified Injection Molding Grade for Sanitary Seals
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 400501S SBS Based Material, 50A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 420451S SBS Based Material, 45D Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 500600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Translucent
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 500750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Translucent
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 500850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Translucent
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 502350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 502550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 502750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 502900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 5049-110 TPE, Modified Injection Molding Grade for Auto Mud Flaps
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 600750S SEBS Based Material, Filled Qualities, 75A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 602300S SEBS Based Material, Filled Qualities, 30A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 602750S SEBS Based Material, Filled Qualities, 75A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 650700 TPE, Improved Compression Set and High Temperature Resistance, 70A Hardness
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660400S SEBS Based Material, Semi-Filled Qualities, 40A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 660850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 8004-101 Flame Retardant TPE for Extrusion, Black, Halogen Free
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Natural, Halogen Free
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Injection Molding, Black
Thermoplastic Elastomer, Melt-Processible Rubber
ELASTO UK Dryflex® 600500S SEBS Based Material, Filled Qualities, 50A Hardness, Natural
Thermoplastic Elastomer, Melt-Processible Rubber
HOME