PRODUCT NO.
Category
ExxonMobil Mytex™ AN17K-01
Polypropylene, Molded
ExxonMobil Mytex™ AS23K(W)-01
Polypropylene (PP)
ExxonMobil Mytex™ AS33L(W)-06
Polypropylene (PP)
ExxonMobil Mytex™ AS33L-07VS
Polypropylene (PP)
ExxonMobil Mytex™ AS65KW-1ATM
Polypropylene (PP)
ExxonMobil Mytex™ AS65KW-LGDC
Polypropylene (PP)