Physical Properties Metric English Comments
Density 12.4 - 13.4 g/cc
0.448 - 0.484 lb/in³
China Tungsten YT769 Tungsten Carbide
Of higher impact toughness than YT798, for vertical rough milling cutters, indexable shallow hole drills, saw web and cut off tools for machining of high strength steel and quality alloy steel.Infor..
Density 12.4 g/cc
0.448 lb/in³
China Tungsten YT790 Tungsten Carbide
Better, toughness, wear resistance high impact resistance thermal cracking resistance, and plastic deformation resistance for rough turning ,milling and planning of steel, esp. forgings and castings..