Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 12.4 - 13.4 g/cc | 0.448 - 0.484 lb/in³ | |
China Tungsten YT769 Tungsten Carbide Of higher impact toughness than YT798, for vertical rough milling cutters, indexable shallow hole drills, saw web and cut off tools for machining of high strength steel and quality alloy steel.Infor.. |
|||
Density | 12.4 g/cc | 0.448 lb/in³ | |
China Tungsten YT790 Tungsten Carbide Better, toughness, wear resistance high impact resistance thermal cracking resistance, and plastic deformation resistance for rough turning ,milling and planning of steel, esp. forgings and castings.. |