Hogen Duralloy H20W 78 Tungsten/22 Copper PM Metal Composite
RWMA Class 11 and 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 mater..
Density >= 14.9 g/cc
>= 0.538 lb/in³
Mi-Tech Metals CW78 78 Tungsten/22 Copper PM Metal Composite
RWMA Class 11 and 12.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is ..
Density 14.9 g/cc
0.538 lb/in³
Indium Corp. Indalloy® 178 Au-In Solder Alloy
Extremely hard, high temperature alloy. Stiff alloy.Information provided by the manufacturer, Indium Corporation.
Density 14.9 g/cc
0.538 lb/in³
Wieland Porta PressOver PFM Alloy
High gold alloy for veneering with IMAGINE® h.e. press ceramicApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, acrylic veneeringDental
Density 14.9 g/cc
0.538 lb/in³
CoorsTek ACI-Co6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Density 14.9 g/cc
0.538 lb/in³
ASTM C20
CoorsTek Tungsten Carbide, WC
Information provided by CoorsTek.
Density 14.9 - 15.2 g/cc
0.538 - 0.549 lb/in³
China Tungsten YG4C Cemented Tungsten Carbide for Mining Purposes
For geological prospecting, coal mining, tipping of electric and air drilk; for coal bed and other homogeneous rocks such as non-silicified shale, skyline and rock salt, etc.; and for medium hard sa..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YG6 Tungsten Carbide for Cutting Tools
High wear resistance ,yet lower than YG3 impact and shock resistance higher than YG3X Semi-finishing and finishing of cast irons ,nonferrous metals & alloys and non metallic materials at medium cutt..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YG6 Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YG600 Tungsten Carbide
High red hardness, wear resistance and thermal strength under high temperature. Machining of cast irons. quenched steel. non-ferrous metals and non-metallic materialsInformation provided by China Tu..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YG6A Tungsten Carbide for Cutting Tools
Fine-grained alloy, good; wear resistance. Semi-finishing of chilled cast iron, non-ferrous metals/alloys; semi-finishing and finishing of hardened steel, alloy steel.Information provided by China T..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YG6C Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YG6X Tungsten Carbide for Cutting Tools
Fine grain WC alloy, wear resistance higher than YG6,strength in use close to YG6,Machining of chilled alloy cast irons and refractory alloy steel or finishing of ordinary cast irons.Information pro..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten YGR7 Tungsten Carbide with Rare Earth Additive
High hardness and strength, low friction, good wear resistance. Used as drawing dies for drawing and straightening of steels, non-ferrous metals and the alloy bars and tubings.Information provided b..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten ZK20 Tungsten Carbide
Roughing and semi-finishing of cast iron. chilled cast iron, low alloy cast iron, non-ferrous metals and non-metallic materials.Information provided by China Tungsten
Density 14.9 g/cc
0.538 lb/in³
CMW® ELKONITE 20SB tungsten, silver
ELKONITE® 20SB is made by a "press-sinter" method with a small addition of nickel used to activate the sintering. Because of fewer steps in manufacture this material is more economical than the Elk..
Density 14.9 g/cc
0.538 lb/in³
China Tungsten ZK10 Tungsten Carbide
It's belong to the fine grain grade. excellent wear resistance. Finishing of cast iron. non-ferrous metals, non-metailic materials and hardened steel. Also suitable for turning and milling.Informati..