Polymer Property : Density = 0.000538 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.