Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.000686 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0190 - 0.100 g/cc
0.000686 - 0.00361 lb/in³
Pressurized batch pre-foamer; Usual Use
NOVA Chemicals Gedexcel® 54B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product and reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, an..
Density 0.0190 - 0.0400 g/cc
0.000686 - 0.00145 lb/in³
Pressurized batch pre-foamer; Usual Use
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
Density 0.0190 - 0.0400 g/cc
0.000686 - 0.00145 lb/in³
Density range normally used
Polimeri Europa Extir® B 2000 Expandable Polystyrene, Fast Molding  (discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l.Processing technology used for Type B 2000 is: Molding, Vacuum.Specific characteristics: Goo..
Density 0.0190 - 0.0350 g/cc
0.000686 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® PD D 2000 AE Expandable Polystyrene, Fast Molding Flame Retardant  (discontinued **)<
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l. Minimum apparent density on a continuous pre-expander is 20 g/l.Processing technology used..
Density >= 0.0190 g/cc
>= 0.000686 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
Ineos Nova Styrocell® M742C Expandable Polystyrene
A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma..
Density 0.0190 - 0.0400 g/cc
0.000686 - 0.00145 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova Styrocell® M742C Expandable Polystyrene
A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma..
Density 0.0190 g/cc
0.000686 lb/in³
45 second cycle time
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding
Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a..
Density 0.0190 g/cc
0.000686 lb/in³
core density
Ultracor® UKF-85-1/4-1.5 Honeycomb Core Material
Construction: ±45° K49 108. Fiber: Kevlar® K49. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD23 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0260 g/cc
0.000686 - 0.000939 lb/in³
sheet density
Zotefoams Plastazote® LD24FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0260 g/cc
0.000686 - 0.000939 lb/in³
sheet density
Zotefoams Plastazote® LD24FMSV Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0250 g/cc
0.000686 - 0.000903 lb/in³
sheet density
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0190 - 0.0350 g/cc
0.000686 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® C 3000 Expandable Polystyrene, Fast Molding  (discontinued **)
Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l.Processing technology used for Type C 3000 is: Molding, Vacuum.Specific characteristics: High t..