Polymer Property : Density = 0.000867 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0180 - 0.0240 g/cc
0.000650 - 0.000867 lb/in³
sheet density
Zotefoams Plastazote® LD18 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0180 - 0.0240 g/cc
0.000650 - 0.000867 lb/in³
sheet density
Zotefoams Plastazote® LD18SC Low Density Polyethylene Foam, Small Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..