Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0290 g/cc | 0.00105 lb/in³ | core density |
Ultracor® UKF-68-3/8-2.0 Honeycomb Core Material Construction: ±45° K49 120. Fiber: Kevlar® K49. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures. It is expected that it will be.. |
|||
Density | 0.0290 - 0.0390 g/cc | 0.00105 - 0.00141 lb/in³ | sheet density |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0290 g/cc | 0.00105 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |