Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0352 g/cc | 0.00127 lb/in³ | |
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |