Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0570 - 0.0740 g/cc | 0.00206 - 0.00267 lb/in³ | sheet density |
Zotefoams Evazote® VA65 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |