Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.102 g/cc | 0.00368 lb/in³ | |
Zoltek Panex 35® Carbon Felt Carbon FeltApplications include: Thermal, Corrosive, or Conductive applications |
|||
Density | 0.102 - 0.112 g/cc | 0.00368 - 0.00405 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |