Polymer Property : Density = 0.00492 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.131 - 0.136 g/cc
0.00475 - 0.00492 lb/in³
Free Rise Density
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio..