Polymer Property : Density = 0.00553 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.153 g/cc
0.00553 lb/in³
apparent nominal; ASTM C271
3A Composites Core Materials BALTEK® SB.100 Structural End-Grain Balsa
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b..