Polymer Property : Density = 0.00975 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.230 - 0.270 g/cc
0.00831 - 0.00975 lb/in³
3M K25 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.230 - 0.270 g/cc
0.00831 - 0.00975 lb/in³
ISO 845-88
Eurofoam Porocell 251 GR NBR/PVC Foam
Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof..