Density 0.340 g/cc
0.0123 lb/in³
True Density as as measured by gas displacement
Potters Industries Sphericel® 34P30 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
Density 0.340 - 0.400 g/cc
0.0123 - 0.0145 lb/in³
3M K37 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..