Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.481 g/cc | 0.0174 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Density | 0.481 g/cc | 0.0174 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Density | 0.481 g/cc | 0.0174 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Density | 0.481 g/cc | 0.0174 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura.. |
|||
Density | >= 0.481 g/cc | >= 0.0174 lb/in³ | |
Monmouth Rubber & Plastics Bondaflexâ„¢ B33CS Sponge Neoprene Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.481 - 0.641 g/cc | 0.0174 - 0.0231 lb/in³ | Dry |
Unifrax Fiberfrax® Vari-Form™ A Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Density | 0.481 - 0.545 g/cc | 0.0174 - 0.0197 lb/in³ | |
Engineered Syntactic Systems MZ-32 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Density | <= 0.481 g/cc | <= 0.0174 lb/in³ | |
Engineered Syntactic Systems SF-30 Subsea Syntactic Void Filler SF-30 is a low cost, low density syntactic formulated to serve as a void filler for shallow water subsea applications. The material is provided as a three-part kit that is mixed and poured into any .. |
|||
Density | 0.481 g/cc | 0.0174 lb/in³ | |
Trelleborg AEM Eccofloat® EL-30/2000 Syntactic Foam EL Grade epoxy syntactic foams are the material of choice for manufacturing manned and unmanned submersibles because of their density range and ability to withstand exposure to diesel fuels and hydr.. |
|||
Density | 0.481 g/cc | 0.0174 lb/in³ | ASTM D1622 |
Touchstone CFOAM® 30 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |