Polymer Property : Density = 0.0210 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0210 g/cc
0.000759 lb/in³
Expected from batch expansion
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength..
Density 0.0210 - 0.0350 g/cc
0.000759 - 0.00126 lb/in³
Polimeri Europa Extir® F 1111 Expandable Polystyrene  (discontinued **)
Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont..
Density 0.0210 - 0.0350 g/cc
0.000759 - 0.00126 lb/in³
Density range normally used
Polimeri Europa Extir® PD F 1111 Expandable Polystyrene, Special Purpose  (discontinued **)
Particle size range is 0.2 - 0.5 mm. Minimum apparent density on a discontinuous pre-expander is 20 g/l. Minimum apparent density on a continuous pre-expander is 24 g/l.Processing technology used ..
Density 0.0210 g/cc
0.000759 lb/in³
2.4 minute residence time pre-expander
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
Density 0.0210 g/cc
0.000759 lb/in³
1 minute residence time pre-expander
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the..
Density 0.0210 - 0.0280 g/cc
0.000759 - 0.00101 lb/in³
sheet density
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..