Physical Properties Metric English Comments
Density 0.620 - 0.620 g/cc

@Temperature 50.0 - 50.0 °C
0.0224 - 0.0224 lb/in³

@Temperature 122 - 122 °F
Average value: 0.620 g/cc Grade Count:1
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..