Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.670 g/cc | 0.0242 lb/in³ | Foamed Density; ISO 1183 |
Stir SpA Z 2002 AT (PVC) Application: Foamed intersoleInformation provided by STIR SpA |
|||
Density | 0.671 g/cc @Temperature 15.0 °C |
0.0242 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ Isohexane Dearomatized Fluid Availability: Africa & Middle East, Asia Pacific and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 15 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | |
DuPont™ Nomex® E56 Paper, 20 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | ASTM C134 |
BNZ Materials BNZP-25L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.671 g/cc | 0.0242 lb/in³ | |
3M 75 Repositionable Spray Adhesive Adhesive that provides tape-like bonds on many lightweight materials. It adheres in seconds, yet has an extra-ling tack range that allows you to life and reposition materials.Features:This adhesive .. |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | |
Henkel SynCore 9823.1 Syntactic Film Toughened, low density syntactic core, superior moisture resistance, co-curable with a variety of 250°F / 121°C curing epoxy prepregs. |
|||
Density | 0.670 g/cc | 0.0242 lb/in³ | |
Henkel SynCore 9872.1 Syntactic Film Toughened, low density syntactic core, superior moisture resistance, co-curable with a wide variety of 350°F / 177°C curing epoxy prepregs. |