Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
CMT Materials HYTAC® B1X High Durability Thermoplastic Syntactic
HYTAC-B1X is the first plug assist material to combine the toughness of an engineered thermoplastic with the low thermal conductivity of syntactic foam. Plug assist made from HYTAC-B1X will resist ..