Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.747 g/cc @Temperature 15.0 °C |
0.0270 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Exxsol™ DSP100/160 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Density | 0.748 g/cc @Temperature 15.0 °C |
0.0270 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Isopar™ G (EU) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu.. |