Density 0.779 g/cc

@Temperature 20.0 °C
0.0281 lb/in³

@Temperature 68.0 °F
LyondellBasell TEBOL® 99 High Purity TBA, Tertiary butyl alcohol
Information provided by Lyondell.
Density 0.779 g/cc
0.0281 lb/in³
3M Hi-Tack 76 Spray Adhesive
Industrial aerosol spray adhesive with high tack for one surface bonding applications.Features:It can effectively bond many hard to hold materials such as polyethylene and polypropyleneIt can also b..
Density 0.779 g/cc
0.0281 lb/in³
3M Super 77™ Spray Adhesive
A high tack, high coverage and fast drying adhesiveFeatures:A high tack, high coverage fast drying, transparent adhesive for permanently attaching foils, carpeting, many lightweight foams, permanent..
Density 0.779 g/cc
0.0281 lb/in³
3M Citrus Base Cleaner Aerosol
3M™ Citrus Base Cleaner is a liquid cleaner/degreaser used to help dissolve and remove dirt, grease, tar, and many non-curing type adhesives. It can also be used in some cases to degrease substrate..
Density 0.779 g/cc
0.0281 lb/in³
BASF N-Butyl Vinyl Ether
Formula: C6H12OCAS: 11-34-2Description: N-Butyl vinyl ether is a colorless to yellow liquid, with an ether-like odor. It is sparingly soluble in water.Synonyms: NBVE, 1-(Vinyloxy)butane, 1-(Ethenyl..
Density 0.779 g/cc
0.0281 lb/in³
3M Super 77™ Cylinder Spray Adhesive
A high tack, high coverage and fast drying adhesiveFeatures:A high tack, high coverage fast drying, transparent adhesive for permanently attaching foils, carpeting, many lightweight foams, permanent..