Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.810 - 0.813 g/cc | 0.0293 - 0.0294 lb/in³ | |
BASF N-Butanol Formula: C4H10OCAS: 71-36-3Description: n-Butanol is a clear, mobile, neutral liquid with a characteristic odor. It is miscible with all common solvents, e.g., alcohols, ketones, aldehydes, ethers, .. |