Polymer Property : Density = 0.0295 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.785 - 0.817 g/cc
0.0284 - 0.0295 lb/in³
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic
HYTAC-FLXT is a unique material, combining the toughness and higher friction of FLX with improved release characteristic through PTFE impregnation. The result is a new, tough syntactic with just th..