Density 0.9385 g/cc
0.03391 lb/in³
ASTM D1505
Petromont 7001 Medium Density Polyethylene Resin
Petromont HDPE 7001 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusi..