Physical Properties Metric English Comments
Density 0.9978 g/cc
0.03605 lb/in³
BASF Polyetheramine D 2000
Description: Polyethermine D 2000 is a yellowish liquid, with an emine-like odor. It is partly miscible with water and other solvents.Applications: Intermediate used in the production of: Plastics, ..