Polymer Property : Density = 0.036254 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.0035 g/cc

@Temperature 15.0 °C
0.036254 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Mobil Jet Oil II
Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combina..
Density 1.0035 g/cc

@Temperature 15.0 °C
0.036254 lb/in³

@Temperature 59.0 °F
ASTM D4052
ExxonMobil Mobil Jet Oil II
Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combina..