Density 1.023 g/cc
0.03696 lb/in³
Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam
STRUKSILON 8120 was developed as universal silicone stabilizer of high potency for the production of conventional as well as flame retardant flexible polyurethane slabstock foam based on polyether p..
Density 1.023 g/cc
0.03696 lb/in³
STN 64 0111
Plastcom SLOVALEN PH 51 T 15 Polypropylene Homopolymer, 15% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 15% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application ..