Polymer Property : Density = 0.03710 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.027 g/cc
0.03710 lb/in³
CRP Technology Windform® FX Polyamide Composite
Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive..
Density 1.027 g/cc
0.03710 lb/in³
ASTM D792
Aclo Accutech Polypropylene Homopolymer HP0339M20CL Mica Reinforced Coupled