Physical Properties Metric English Comments
Density 1.029 g/cc
0.03717 lb/in³
ISO 1183
Styrolution Polystyrol 485 I GR 2 PS
Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro..
Density 1.029 g/cc
0.03717 lb/in³
ISO 1183
Styrolution Polystyrol ESCRimo PS
Description: Polystyrol ESCRimo is a high-impact polystyrene grade with an improved stress cracking resistance compared to conventional high-impact polystyrene.Applications: Due to its superior envi..