Polymer Property : Density = 0.03811 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.055 g/cc
0.03811 lb/in³
ISO 1183
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade
Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food..
Density 1.055 g/cc
0.03811 lb/in³
Dow BETAFOAM™ 87120 Polyether / Polyol Blend
BETAFOAM™ 87120 is a component used to make low density, all water blown rigid polyurethane foam.Information provided by Dow
Density 1.055 g/cc
0.03811 lb/in³
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound
FormulationNordel® IP 4570